The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 08, 2020

Filed:

Jun. 19, 2017
Applicant:

Ngk Spark Plug Co., Ltd., Nagoya-shi, Aichi, JP;

Inventors:

Jun Moteki, Seto, JP;

Yusuke Katsu, Komaki, JP;

Takeshi Mitsuoka, Konan, JP;

Assignee:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/117 (2006.01); C04B 35/44 (2006.01); C04B 35/626 (2006.01); C04B 35/64 (2006.01); C09K 11/77 (2006.01); C04B 35/10 (2006.01);
U.S. Cl.
CPC ...
C04B 35/117 (2013.01); C04B 35/10 (2013.01); C04B 35/44 (2013.01); C04B 35/6261 (2013.01); C04B 35/62625 (2013.01); C04B 35/62695 (2013.01); C04B 35/64 (2013.01); C09K 11/7774 (2013.01); C04B 35/62605 (2013.01); C04B 2235/3217 (2013.01); C04B 2235/3222 (2013.01); C04B 2235/3224 (2013.01); C04B 2235/3225 (2013.01); C04B 2235/3227 (2013.01); C04B 2235/3229 (2013.01); C04B 2235/3286 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/5445 (2013.01); C04B 2235/602 (2013.01); C04B 2235/604 (2013.01); C04B 2235/6581 (2013.01); C04B 2235/762 (2013.01); C04B 2235/764 (2013.01); C04B 2235/77 (2013.01); C04B 2235/785 (2013.01); C04B 2235/786 (2013.01); C04B 2235/96 (2013.01); C04B 2235/9607 (2013.01); C04B 2235/9646 (2013.01);
Abstract

The durability of a ceramic sintered body is improved, and a reduction in its light emission intensity and the occurrence of a chromaticity variation are suppressed. The ceramic sintered body contains alumina and a compound represented by M1M2M3O. The volume percent of the compound in the ceramic sintered body is from 3% to 70% inclusive. The ratio of the intensity of XRD from a complex oxide of aluminum and M2 to the intensity of XRD from the compound in the ceramic sintered body is less than 0.05. The average grain diameter of the alumina contained in the ceramic sintered body is from 0.30 (μm) to 3.00 (μm) inclusive. M1 is at least one selected from Sc, Y, and lanthanoid elements, and M2 is at least one selected from lanthanoid elements except any lanthanoid element selected for M1. M3 is at least one of Al and Ga, and X is from 0.003 to 0.500 inclusive.