The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Sep. 01, 2020
Filed:
Aug. 25, 2015
Sumitomo Metal Mining Co., Ltd., Tokyo, JP;
Hideharu Okami, Niihama, JP;
SUMITOMO METAL MINNING CO., LTD., Tokyo, JP;
Abstract
[Object] Provided are an electrode substrate film in which a circuit pattern formed of a metal thin line is less visible even under highly bright illumination, and a laminate film applied to the same. [Solving Means] An electrode substrate film with a transparent substrateand a metal laminate thin line includes a metal absorption layerwith a film thickness of 20 nm to 30 nm inclusive as a first layer, and a metal layeras a second layer, counted from the transparent substrate side, the laminate thin line having a line width of 20 μm or less. Optical constants of the metal absorption layer in a visible wavelength range (400 to 780 nm) satisfy conditions that a refractive index is 2.0 to 2.2 and an extinction coefficient is 1.8 to 2.1 at a wavelength of 400 nm, the refractive index is 2.4 to 2.7 and the extinction coefficient is 1.9 to 2.3 at a wavelength of 500 nm, the refractive index is 2.8 to 3.2 and the extinction coefficient is 1.9 to 2.5 at a wavelength of 600 nm, the refractive index is 3.2 to 3.6 and the extinction coefficient is 1.7 to 2.5 at a wavelength of 700 nm, and the refractive index is 3.5 to 3.8 and the extinction coefficient is 1.5 to 2.4 at a wavelength of 780 nm. An average reflectance in the visible wavelength range attributed to reflection at an interface between the transparent substrate and the metal absorption layer is 20% or less, and a difference between a highest reflectance and a lowest reflectance in the visible wavelength range is 10% or less.