The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 01, 2020

Filed:

Jul. 06, 2018
Applicant:

Petrochina Company Limited, Beijing, CN;

Inventors:

Jianhui Luo, Beijing, CN;

Zongtao Zhang, Beijing, CN;

Baoliang Peng, Beijing, CN;

Runwei Wang, Beijing, CN;

Lipeng He, Beijing, CN;

Pingmei Wang, Beijing, CN;

Bin Ding, Beijing, CN;

Ying Wang, Beijing, CN;

Xiangfei Geng, Beijing, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C01B 39/38 (2006.01); B01J 29/40 (2006.01); C01B 39/02 (2006.01);
U.S. Cl.
CPC ...
C01B 39/026 (2013.01); B01J 29/40 (2013.01); C01B 39/38 (2013.01); B01J 2229/12 (2013.01); B01J 2229/14 (2013.01); B01J 2229/32 (2013.01); B01J 2229/34 (2013.01); B01J 2229/38 (2013.01); B01J 2229/40 (2013.01); C01P 2002/72 (2013.01); C01P 2004/03 (2013.01); C01P 2004/04 (2013.01); C01P 2004/34 (2013.01); C01P 2004/36 (2013.01); C01P 2004/90 (2013.01); C01P 2006/16 (2013.01);
Abstract

The present invention provides an amphiphilic molecular sieve containing a hydrophilic group on the outside and a lipophilic group on the inside and a production method thereof. The production method comprises: dispersing the ZSM-5 spherical nano-molecular sieve into toluene, adding thereto an organosilane containing a hydrophilic group and reacting at 40-80° C. for 2-16 h, to obtain a molecular sieve containing a hydrophilic group; placing the molecular sieve containing a hydrophilic group in an aqueous solution of sodium hydroxide and reacting at 50-90° C. for 10-50 min, to obtain a molecular sieve containing a hydrophilic group on the outside; dispersing the molecular sieve containing a hydrophilic group on the outside into toluene, adding thereto an organosilane containing a lipophilic group and reacting at 40-80° C. for 2-12 h, to obtain the amphiphilic molecular sieve containing a hydrophilic group on the outside and a lipophilic group on the inside. The present invention also provides an amphiphilic molecular sieve obtained by the above production method, which contains a hydrophilic group on the outside and a lipophilic group on the inside.