The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 25, 2020

Filed:

Jun. 14, 2017
Applicant:

Toray Industries, Inc., Tokyo, JP;

Inventors:

Atsushi Sawamoto, Otsu, JP;

Masanori Sueoka, Otsu, JP;

Kazuma Matsui, Otsu, JP;

Kohei Sato, Otsu, JP;

Akimitsu Tsukuda, Otsu, JP;

Junji Michizoe, Gumi, KR;

Do Kyun Kim, Gumi, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 27/34 (2006.01); B32B 27/00 (2006.01); C08J 7/046 (2020.01); C09D 7/20 (2018.01); B32B 7/02 (2019.01); C08J 7/04 (2020.01); B32B 27/28 (2006.01); B32B 38/00 (2006.01);
U.S. Cl.
CPC ...
B32B 27/34 (2013.01); B32B 7/02 (2013.01); B32B 27/00 (2013.01); B32B 27/281 (2013.01); C08J 7/042 (2013.01); C08J 7/046 (2020.01); C09D 7/20 (2018.01); B32B 2038/0052 (2013.01); B32B 2307/536 (2013.01); B32B 2457/208 (2013.01); C08J 2379/08 (2013.01);
Abstract

A laminated film includes, at least on one side thereof, a layer containing a hardening resin, having a total thickness of 1 to 100 μm, a light transmittance of 70% or more at a wavelength of 400 nm, a Young's modulus of 5 GPa or more when applying a nanoindenter to make a 1 μm depression in the thickness direction into the surface of the hardening layer, and undergoing a rate of deformation of 500 ppm or less after applying a stress of 0.5 MPa for 30 minutes.