The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 04, 2020

Filed:

Jan. 30, 2019
Applicant:

Nova Chemicals (International) S.a., Fribourg, CH;

Inventors:

Xiaoliang Gao, Calgary, CA;

Vasily Simanzhenkov, Calgary, CA;

Marie Barnes, Calgary, CA;

David Sullivan, Calgary, CA;

Hanna Drag, Calgary, CA;

Yoonhee Kim, Calgary, CA;

Perry de Wit, Calgary, CA;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 27/057 (2006.01); B01J 37/03 (2006.01); B01J 37/00 (2006.01); B01J 37/10 (2006.01); B01J 37/08 (2006.01); B01J 35/02 (2006.01); C07C 2/84 (2006.01); B01J 23/00 (2006.01); B01J 23/22 (2006.01); B01J 23/28 (2006.01); B01J 37/04 (2006.01); B01J 37/06 (2006.01); C07C 5/48 (2006.01); C07C 2/82 (2006.01); C07C 5/32 (2006.01);
U.S. Cl.
CPC ...
B01J 27/0576 (2013.01); B01J 23/002 (2013.01); B01J 23/22 (2013.01); B01J 23/28 (2013.01); B01J 35/023 (2013.01); B01J 37/0009 (2013.01); B01J 37/0018 (2013.01); B01J 37/0045 (2013.01); B01J 37/0063 (2013.01); B01J 37/03 (2013.01); B01J 37/04 (2013.01); B01J 37/06 (2013.01); B01J 37/08 (2013.01); B01J 37/088 (2013.01); B01J 37/10 (2013.01); C07C 2/84 (2013.01); C07C 5/48 (2013.01); B01J 2523/00 (2013.01); C07C 2/82 (2013.01); C07C 5/32 (2013.01); C07C 2523/20 (2013.01); C07C 2523/22 (2013.01); C07C 2523/28 (2013.01); C07C 2523/32 (2013.01);
Abstract

A process for preparing an oxidative dehydrogenation catalyst or oxidative dehydrogenation catalyst precursor that includes mixing solutions of molybdenum and tellurium at a pH from about 3.3 to 7.5; adjusting the pH of the resulting solution back to about 5 and adding VOSOand adding a solution of NbOand oxalic acid and treating the resulting precursor slurry in a controlled pressure hydrothermal process to obtain the catalyst.