The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2020

Filed:

Jun. 09, 2016
Applicant:

Hitachi Automotive Systems, Ltd., Hitachinaka-shi, Ibaraki, JP;

Inventors:

Xudong Zhang, Tokyo, JP;

Shinya Okamoto, Tokyo, JP;

Nobuaki Kobayashi, Hitachinaka, JP;

Takahiro Saito, Hitachinaka, JP;

Akihiro Yamazaki, Hitachinaka, JP;

Assignee:

Hitachi Automotive Systems, Ltd., Hitachinaka-shi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
F02M 61/16 (2006.01); B23K 26/34 (2014.01); B23K 26/064 (2014.01); B23K 26/354 (2014.01); B23K 26/08 (2014.01); B23K 103/04 (2006.01); B23P 15/00 (2006.01); F02M 51/06 (2006.01);
U.S. Cl.
CPC ...
F02M 61/166 (2013.01); B23K 26/064 (2015.10); B23K 26/0823 (2013.01); B23K 26/34 (2013.01); B23K 26/354 (2015.10); F02M 61/16 (2013.01); B23K 2103/05 (2018.08); B23P 15/001 (2013.01); F02M 51/0664 (2013.01); F02M 61/168 (2013.01);
Abstract

There is provided a manufacturing method of a hollow composite magnetic member having weakened magnetism in a portion of a ferromagnetic hollow member, the method includes: a step of forming a weak-magnetic area having weakened magnetism by melting and mixing a Ni-containing material and the hollow member by continuously supplying the Ni-containing material to a portion of the hollow member and heating the irradiation area having a line segment shape with the laser beam. Accordingly, since it is possible to prevent drop of a local portion of a hollow ferromagnetic pipe from being easily generated by a weak-magnetization treatment, to greatly reduce deformation generated by laser irradiation, and it becomes unnecessary to adjust the shielding gas pressure inside the pipe, the weak-magnetization treatment can be performed with higher efficiency and higher quality.


Find Patent Forward Citations

Loading…