The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2020

Filed:

May. 12, 2017
Applicant:

Saint-gobain Glass France, Courbevoie, FR;

Inventors:

Stéphane Berard, Mouy, FR;

Alexandre Hennion, Venette, FR;

Philippe Frebourg, Senlis, FR;

Assignee:

SAINT-GOBAIN GLASS FRANCE, Courbevoie, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
E06B 3/673 (2006.01); C03B 27/044 (2006.01); B32B 17/10 (2006.01); C03B 27/04 (2006.01); C03B 27/004 (2006.01); C03B 23/035 (2006.01); C03B 23/03 (2006.01); C03B 23/025 (2006.01); C03B 23/023 (2006.01); B60J 7/043 (2006.01); B60J 1/00 (2006.01); C03B 33/07 (2006.01);
U.S. Cl.
CPC ...
E06B 3/673 (2013.01); B32B 17/10036 (2013.01); B32B 17/1099 (2013.01); B32B 17/10293 (2013.01); B32B 17/10761 (2013.01); B32B 17/10981 (2013.01); B60J 1/001 (2013.01); B60J 7/043 (2013.01); C03B 23/023 (2013.01); C03B 23/0252 (2013.01); C03B 23/0258 (2013.01); C03B 23/03 (2013.01); C03B 23/0352 (2013.01); C03B 27/004 (2013.01); C03B 27/0404 (2013.01); C03B 27/0413 (2013.01); C03B 27/0442 (2013.01); C03B 33/078 (2013.01); Y10T 29/49826 (2015.01); Y10T 428/24322 (2015.01); Y10T 428/24612 (2015.01); Y10T 428/24628 (2015.01);
Abstract

A laminated includes two bent glass substrates, a polymer interlayer between the glass substrates, and a notch or orifice cut in an entire thickness of the glazing. The glazing includes a border of compressive edge stresses obtained by general controlled cooling of the substrates in a paired state so that compressive stresses are generated at the border, and a local compression zone, different from the border, and obtained by local controlled cooling of a local area of a main surface of the glazing so that compressive stresses are generated in theid local compression zone. The notch or orifice is located in the local compression zone and made in the substrates in a paired state after forming the local compression zone so that cut contours of the substrates in the notch or orifice have a perfect superposition. The compressive edge stresses of the cut contours are greater than 4 MPa.