The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2020

Filed:

Aug. 28, 2012
Applicants:

Daniel Gantenbein, Elnesvagen, NO;

Joachim Schoelkopf, Killwangen, CH;

Patrick A. C. Gane, Rothrist, CH;

Inventors:

Daniel Gantenbein, Elnesvagen, NO;

Joachim Schoelkopf, Killwangen, CH;

Patrick A. C. Gane, Rothrist, CH;

Assignee:

Omya International AG, Oftringen, CH;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C09C 3/10 (2006.01); C09C 1/02 (2006.01); D21H 19/42 (2006.01); D21H 17/00 (2006.01); D21H 17/69 (2006.01); A01N 59/06 (2006.01); D21H 17/25 (2006.01);
U.S. Cl.
CPC ...
C09C 3/10 (2013.01); A01N 59/06 (2013.01); C09C 1/021 (2013.01); D21H 17/00 (2013.01); D21H 17/25 (2013.01); D21H 17/69 (2013.01); D21H 17/74 (2013.01); D21H 19/42 (2013.01); C01P 2004/50 (2013.01); C01P 2004/62 (2013.01); C01P 2006/22 (2013.01); C01P 2006/60 (2013.01);
Abstract

The present invention relates to a process for preparing self-binding pigment particles comprising the following steps: a) providing an aqueous mineral pigment material suspension; b) providing at least one polymeric binder, wherein the binder comprises at least one modified polysaccharide having a degree of carboxylation in the range of 0.4 to 2.0 and having an intrinsic viscosity in the range of >300 to 500 ml/g, c) mixing the binder of step b) with the aqueous mineral pigment material suspension of step a) and adjusting the solids content of the obtained suspension so that it is >45 to 95 wt.-%, preferably from 45 to 80 wt.-%, based on the total weight of the suspension, and d) grinding the aqueous mineral material suspension of step c).