The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2020

Filed:

Mar. 07, 2017
Applicant:

Haldor Topsøe A/s, Kgs. Lyngby, DK;

Inventors:

Poul Erik Højlund Nielsen, Fredensborg, DK;

Rasmus Munksgård Nielsen, Humlebæk, DK;

Lived J. Lemus-Yegres, Copenhagen S, DK;

Assignee:

HALDOR TOPSØE A/S, Kgs. Lyngby, DK;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 27/051 (2006.01); B01J 27/043 (2006.01); B01J 27/047 (2006.01); B01J 27/30 (2006.01); C07C 5/32 (2006.01); B01J 37/20 (2006.01); B01J 37/18 (2006.01); B01J 37/02 (2006.01); B01J 27/04 (2006.01); B01J 38/18 (2006.01); B01J 38/64 (2006.01); B01J 35/00 (2006.01); B01J 35/10 (2006.01);
U.S. Cl.
CPC ...
B01J 27/0515 (2013.01); B01J 27/04 (2013.01); B01J 27/043 (2013.01); B01J 27/047 (2013.01); B01J 27/051 (2013.01); B01J 27/30 (2013.01); B01J 37/0201 (2013.01); B01J 37/18 (2013.01); B01J 37/20 (2013.01); B01J 38/18 (2013.01); B01J 38/64 (2013.01); C07C 5/321 (2013.01); C07C 5/322 (2013.01); B01J 35/006 (2013.01); B01J 35/1042 (2013.01); C07C 2523/75 (2013.01); C07C 2527/04 (2013.01); C07C 2527/043 (2013.01); C07C 2527/047 (2013.01); C07C 2527/049 (2013.01); C07C 2527/051 (2013.01); Y02P 20/52 (2015.11); Y02P 20/584 (2015.11);
Abstract

A catalyst for the dehydrogenation of alkanes to alkenes comprises a catalytically active material supported on a carrier, wherein the catalytically active material is a metallic sulfide (MeS) comprising Fe, Co, Ni, Cu, Mo or W or any combination of two or more metals selected from Pb, Sn, Zn, Fe, Co, Ni, Cu, Mo and W. The catalyst is regenerated in several steps. The dehydrogenation is carried out at a temperature between 450 and 650° C. and a pressure from 0.9 bar below ambient pressure to 5 bar above ambient pressure.