The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jul. 21, 2020
Filed:
Apr. 10, 2018
Applicant:
Asustek Computer Inc., Taipei, TW;
Inventor:
Fei-Lin Yang, Taipei, TW;
Assignee:
ASUSTEK COMPUTER INC., Taipei, TW;
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 2/02 (2006.01); B32B 15/20 (2006.01); B32B 27/34 (2006.01); B32B 15/09 (2006.01); B32B 15/085 (2006.01); B32B 15/088 (2006.01); B32B 7/12 (2006.01); B32B 15/02 (2006.01); C04B 37/00 (2006.01); H01M 10/0525 (2010.01); B32B 27/12 (2006.01); B32B 27/32 (2006.01); B32B 5/02 (2006.01); B32B 27/36 (2006.01);
U.S. Cl.
CPC ...
H01M 2/0287 (2013.01); B32B 5/028 (2013.01); B32B 7/12 (2013.01); B32B 15/02 (2013.01); B32B 15/085 (2013.01); B32B 15/088 (2013.01); B32B 15/09 (2013.01); B32B 15/20 (2013.01); B32B 27/12 (2013.01); B32B 27/32 (2013.01); B32B 27/34 (2013.01); B32B 27/36 (2013.01); C04B 37/005 (2013.01); H01M 2/0277 (2013.01); H01M 2/0285 (2013.01); C04B 2237/04 (2013.01); C04B 2237/062 (2013.01); C04B 2237/083 (2013.01); H01M 10/0525 (2013.01);
Abstract
The invention discloses a packaging film for a battery. The packaging film for the battery comprises an electrolyte-resistant layer, a protective layer, and a high-rigidity material layer. The high-rigidity material layer is located between the electrolyte-resistant layer and the protective layer. The high-rigidity material layer comprises a substrate layer and at least one cermet film. The substrate layer has two surfaces facing the electrolyte-resistant layer and the protective layer respectively. The at least one cermet film is located on at least one of the two surfaces of the substrate layer.