The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 23, 2020

Filed:

Dec. 05, 2015
Applicants:

Truetzschler Gmbh & Co. KG, Moenchengladbach, DE;

Dsm Ip Assets B.v., Te Heerlen, NL;

Inventors:

Lassad Nasri, Winterthur, CH;

Roman Stepanyan, AA Echt, NL;

Martinus Joseph Maria Keulers, AA Echt, NL;

Assignees:

TRUETZSCHLER GMBH & CO. KG, Moenchengladbach, DE;

DSM IP ASSETS B.V., Te Heerlen, NL;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
D01D 5/16 (2006.01); C08G 69/46 (2006.01); D01D 4/02 (2006.01); D01F 6/60 (2006.01); D02G 3/02 (2006.01); D02G 3/44 (2006.01); D02J 1/22 (2006.01);
U.S. Cl.
CPC ...
D01D 5/16 (2013.01); C08G 69/46 (2013.01); D01D 4/02 (2013.01); D01F 6/60 (2013.01); D02G 3/02 (2013.01); D02G 3/446 (2013.01); D02J 1/228 (2013.01); D02J 1/229 (2013.01);
Abstract

A process and an apparatus for production of a low-shrinkage aliphatic polyamide fibre, in which polyamide is extruded through a spinneret to form filaments, then cooled and combined to form at least one yarn. The at least one yarn is subjected to drawing between the spinneret and a pair of inlet rolls, then in a further multi-stage drawing step is subjected to 4-fold to 6-fold drawing by pairs of draw rolls. The pairs of draw rolls successively heat the yarn and at least the last pair of draw rolls has a temperature of 5° C. to 20° C. below the melting point of the yarn. The yarn is relaxed by from 6% to 10% in a subsequent at least three-stage relaxation zone and is kept in a temperature range of 5° C. to 15° C. below the melting point of the yarn, and is subsequently wound up on a reel device. The invention further relates to a yarn composed of a low-shrinkage aliphatic polyamide fibre.