The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 23, 2020

Filed:

Aug. 03, 2016
Applicant:

Jinan Shengquan Group Share Holding Co., Ltd., Shandong, CN;

Inventors:

Yilin Tang, Shandong, CN;

Jinzhu Zhang, Shandong, CN;

An Zhang, Shandong, CN;

Feng Luan, Shandong, CN;

Ding Liu, Shandong, CN;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C08K 3/04 (2006.01); D01F 1/09 (2006.01); D01F 6/92 (2006.01); C08L 67/02 (2006.01); D01F 1/10 (2006.01); C08J 5/00 (2006.01); C08J 3/21 (2006.01); B29B 7/90 (2006.01); B29B 9/06 (2006.01); D01D 5/088 (2006.01); B29K 67/00 (2006.01); B29K 507/04 (2006.01);
U.S. Cl.
CPC ...
C08K 3/04 (2013.01); B29B 7/90 (2013.01); B29B 9/065 (2013.01); C08J 3/212 (2013.01); C08J 5/005 (2013.01); C08L 67/02 (2013.01); D01D 5/0885 (2013.01); D01F 1/09 (2013.01); D01F 1/10 (2013.01); D01F 6/92 (2013.01); B29K 2067/003 (2013.01); B29K 2507/04 (2013.01); C08J 2367/02 (2013.01); C08K 2201/011 (2013.01);
Abstract

A polyester material including a composite having a carbon nanostructure, which comprises carbon element, from 0.5 to 4 wt % of a first non-carbon non-oxygen element substance, and from 0 to 4 wt %, of a second non-carbon non-oxygen element. The first non-carbon non-oxygen element is selected from the group consisting of P, Si, Ca, Al and Na; the second non-carbon non-oxygen element is any one selected from the group consisting of Fe, Ni, Mn, K, Mg, Cr, S or Co, or a combination of at least two selected therefrom. The G peak and D peak of the carbon element in the Raman spectrum has a peak height ratio of 1-20 in the composite having a carbon nanostructure.