The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 02, 2020

Filed:

May. 24, 2018
Applicant:

Sumito Metal Mining Co., Ltd., Tokyo, JP;

Inventors:

Hiroyuki Toya, Niihama, JP;

Kensaku Mori, Niihama, JP;

Shin Imaizumi, Niihama, JP;

Kenji Ikeuchi, Niihama, JP;

Toshiyuki Osako, Niihama, JP;

Assignee:
Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/525 (2010.01); C30B 7/14 (2006.01); H01M 4/505 (2010.01); C01G 53/00 (2006.01); H01M 4/04 (2006.01); H01M 4/36 (2006.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
C30B 7/14 (2013.01); C01G 53/006 (2013.01); C01G 53/50 (2013.01); H01M 4/0471 (2013.01); H01M 4/0497 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); C01P 2002/52 (2013.01); C01P 2004/03 (2013.01); C01P 2004/34 (2013.01); C01P 2004/51 (2013.01); C01P 2004/61 (2013.01); C01P 2004/62 (2013.01); C01P 2006/40 (2013.01); H01M 4/366 (2013.01); H01M 10/0525 (2013.01); Y10T 428/2982 (2015.01);
Abstract

Provided are nickel manganese composite hydroxide particles having a small and uniform particle size and having a double structure which enables to obtain a cathode active material having a hollow structure, and a manufacturing method thereof. When obtaining the nickel manganese composite hydroxide by a reaction crystallization, using an aqueous solution for nucleation, which includes at least a metallic compound that contains nickel, a metallic compound that contains manganese and an ammonium ion donor and controlling the pH value that is measured at a standard solution temperature of 25° C. is 10.5 to 12.0, nucleation is performed in an oxidizing atmosphere in which the oxygen concentration is greater than 1% by volume, and then nuclei are grown by switching the atmosphere from the oxidizing atmosphere to a mixed atmosphere of oxygen and inert gas in which the oxygen concentration is 1% by volume or less.