The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 12, 2020

Filed:

Jul. 18, 2018
Applicant:

Panasonic Intellectual Property Management Co., Ltd., Osaka, JP;

Inventors:

Takayuki Ishikawa, Osaka, JP;

Ryuichi Natsui, Osaka, JP;

Kensuke Nakura, Osaka, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/00 (2006.01); H01M 4/36 (2006.01); H01M 4/505 (2010.01); H01M 4/58 (2010.01); H01M 4/525 (2010.01); H01M 4/485 (2010.01); C01G 45/12 (2006.01); C01G 51/00 (2006.01); H01M 4/62 (2006.01); C01G 53/00 (2006.01); H01M 4/02 (2006.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
H01M 4/366 (2013.01); C01G 45/1228 (2013.01); C01G 51/50 (2013.01); C01G 53/50 (2013.01); H01M 4/485 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); H01M 4/5825 (2013.01); H01M 4/62 (2013.01); C01P 2002/72 (2013.01); C01P 2002/74 (2013.01); C01P 2002/76 (2013.01); C01P 2004/80 (2013.01); C01P 2004/84 (2013.01); H01M 10/0525 (2013.01); H01M 2004/028 (2013.01); H01M 2300/0068 (2013.01); H01M 2300/0071 (2013.01);
Abstract

A positive electrode active material contains a lithium composite oxide and a covering material. The lithium composite oxide contains at least one element selected from the group consisting of fluorine, chlorine, nitrogen, and sulfur. The lithium composite oxide has a crystal structure that belongs to space group C2/m. The ratio I/Iof a first integrated intensity Iof a first peak corresponding to a (003) plane to a second integrated intensity Iof a second peak corresponding to a (104) plane in an XRD pattern of the lithium composite oxide satisfies 0.05≤I/I≤0.90. The covering material has an electron conductivity of 10S/m or less.