The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 12, 2020

Filed:

Jan. 19, 2017
Applicant:

Beijing University of Technology, Beijing, CN;

Inventors:

Wei Liu, Beijing, CN;

Mingchaung Tian, Beijing, CN;

Jinshu Wang, Beijing, CN;

Fan Zhou, Beijing, CN;

Yiman Wang, Beijing, CN;

Liran Dong, Beijing, CN;

Yunfei Yang, Beijing, CN;

Quan Zhang, Beijing, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22F 3/105 (2006.01); H01J 9/04 (2006.01); B22F 9/02 (2006.01); B22F 9/22 (2006.01); C22B 34/36 (2006.01); B22F 9/30 (2006.01); H01J 1/28 (2006.01); H01J 19/22 (2006.01); H01J 35/06 (2006.01);
U.S. Cl.
CPC ...
H01J 9/04 (2013.01); B22F 3/105 (2013.01); B22F 9/026 (2013.01); B22F 9/22 (2013.01); B22F 9/30 (2013.01); C22B 34/36 (2013.01); B22F 2003/1054 (2013.01); B22F 2998/10 (2013.01); H01J 1/28 (2013.01); H01J 19/22 (2013.01); H01J 35/06 (2013.01);
Abstract

The present disclosure discloses a preparation method of pressed Scandia-doped dispenser cathode using microwave sintering. Embodiments of the present disclosure include dissolving some nitrates and ammonium metatungstate with deionized water to prepare a homogeneous solution. Precursor powder with uniform size is obtained by spray drying, the precursor powder is decomposed, and two-step reduction may be proceeded to form doped tungsten powder with uniform element distribution. The cathode is prepared by one-time microwave sintering. One-time forming of cathode sintering is realized, and sintering shrinkage and sintering time are reduced significantly. The method has excellent repeatability, and the cathode has a homogeneous structure and excellent emission performance at 950° C.


Find Patent Forward Citations