The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 12, 2020

Filed:

Apr. 14, 2015
Applicant:

Wellbore Integrity Solutions Llc, Houston, TX (US);

Inventors:

Wenhui Jiang, Pearland, TX (US);

Fengxiao Liu, Houston, TX (US);

Alan W. Lockstedt, Magnolia, TX (US);

Doyle Wayne Brinegar, Conroe, TX (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/50 (2006.01); C21D 9/08 (2006.01); C21D 1/00 (2006.01); C21D 6/00 (2006.01); C21D 1/26 (2006.01); C21D 1/56 (2006.01); B23K 9/23 (2006.01); B23K 20/227 (2006.01); B23K 31/02 (2006.01); E21B 17/16 (2006.01); B23K 9/028 (2006.01); B23K 20/12 (2006.01); B23K 103/04 (2006.01); B23K 101/06 (2006.01);
U.S. Cl.
CPC ...
C21D 1/00 (2013.01); B23K 9/0282 (2013.01); B23K 9/23 (2013.01); B23K 20/129 (2013.01); B23K 20/227 (2013.01); B23K 31/02 (2013.01); C21D 1/26 (2013.01); C21D 1/56 (2013.01); C21D 6/00 (2013.01); C21D 9/085 (2013.01); C21D 9/505 (2013.01); E21B 17/16 (2013.01); B23K 2101/06 (2018.08); B23K 2103/04 (2018.08); C21D 2251/04 (2013.01);
Abstract

A heavy weight drill pipe may include a tube body formed of AISI 1340 alloy steel, and first and second tool joints at respective ends of the tube body, and which are formed of an AISI 41XX series alloy steel. The first and second tool joints may be welded to the tube body at a weld line within a weld region. A Charpy impact toughness at the weld line or surrounding weld region may be least 12 ft-lbs. (16.5 N-m). Yield and tensile strengths at the weld line or weld region may be at least 65 ksi (448.0 MPa) and at least 106 ksi (731.0 MPa), respectively. Material properties at the weld line or weld region may be achieved by heat treating after welding. Heat treating may include austenitizing, quenching, and tempering the weld line and/or the surrounding weld region.