The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 28, 2020

Filed:

Aug. 12, 2015
Applicants:

Aledia, Grenoble, FR;

Universite Blaise Pascal-clermont Ii, Clermont Ferrand, FR;

Centre National DE LA Recherche Scientifique, Paris, FR;

Sigma Clermont, Aubiere, FR;

Inventors:

Abdelhay Aboulaich, Clermont-Ferrand, FR;

Geneviève Chadeyron, Cebazat, FR;

Rachid Mahiou, Clermont-Ferrand, FR;

Assignees:

Aledia, Grenoble, FR;

Universite Clermont Auvergne, Clermont Ferrand, FR;

Centre National de la Recherche Scientifique, Paris, FR;

Sigma Clermont, Aubiere, FR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C09K 11/77 (2006.01); C04B 35/505 (2006.01); C04B 35/624 (2006.01); C04B 35/626 (2006.01);
U.S. Cl.
CPC ...
C09K 11/7721 (2013.01); C04B 35/505 (2013.01); C04B 35/624 (2013.01); C04B 35/62645 (2013.01); C04B 35/62695 (2013.01); C09K 11/7774 (2013.01); C04B 2235/95 (2013.01);
Abstract

A method for producing a photo-luminescent material, including the following steps: (1) producing, according to a sol-gel method, a sol and then a gel of first precursors of a first substance from the sol; (2) crushing the gel; (3) optionally, annealing the gel in order to form first particles of the first substance of which the average size is between 1 pm and 20 um; (4) producing a colloidal dispersion of second particles of a second substance, different from the first substance or identical to the first substance, of which the average size is between 5 nm and 400 nm; (5) mixing the colloidal dispersion with the sol in step (1) before forming the gel or with the first particles after step (3); and (6) annealing the mixture obtained in step (5), resulting in an increase in the compactness of the mixture, the average size of the second particles after annealing being between 100 nm and 900 nm. A photo-luminescent material including a mixture of first particles of a first photo-luminescent substance of which the average size is between 1 pm and 20 pm and second particles of a second photo-luminescent substance, different from the first photo-luminescent substance or identical to the first photo-luminescent substance, of which the average size is between 100 nm and 900 nm.