The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 21, 2020

Filed:

Jan. 25, 2016
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Yoshie Obata, Chiba, JP;

Yoshiyasu Kawasaki, Chiba, JP;

Keiji Ueda, Kurashiki, JP;

Shinjiro Kaneko, Chiba, JP;

Takeshi Yokota, Kawasaki, JP;

Kazuhiro Seto, Chiba, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C22C 38/14 (2006.01); C21D 8/02 (2006.01); C23C 2/06 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/60 (2006.01); C22C 38/00 (2006.01); C22C 38/18 (2006.01); C22C 38/16 (2006.01); C23C 2/02 (2006.01); C23C 2/40 (2006.01);
U.S. Cl.
CPC ...
C22C 38/14 (2013.01); C21D 8/0236 (2013.01); C21D 8/0268 (2013.01); C21D 9/46 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/16 (2013.01); C22C 38/18 (2013.01); C22C 38/60 (2013.01); C23C 2/02 (2013.01); C23C 2/06 (2013.01); C23C 2/40 (2013.01); C21D 2211/001 (2013.01); C21D 2211/004 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01); C21D 2211/009 (2013.01);
Abstract

A steel having a composition containing C: more than 0.20% and 0.45% or less, Si: 0.50% to 2.50%, Mn: 2.00% or more and less than 3.50%, and one or two selected from Ti: 0.005% to 0.100% and Nb: 0.005% to 0.100% is hot-rolled and cold-rolled. The steel sheet is heated to 800° C. to 950° C. and cooled to a cooling-end temperature of 350° C. to 500° C. at a cooling rate of 5° C./s or more to form a steel sheet having a microstructure including martensite and bainite phases such that the total proportion of the martensite and bainite phases is 80% or more by volume. The steel sheet is heated to 700° C. to 840° C. and maintained at 700° C. to 840° C., cooled to a cooling-end temperature of 350° C. to 500° C. at a cooling rate of 5 to 50° C./s, and maintained within the above temperature range for 10 to 1800 s.