The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 07, 2020

Filed:

Oct. 21, 2016
Applicants:

Rolls-royce Corporation, Indianapolis, IN (US);

Rolls-royce High Temperature Composites, Inc., Cypress, CA (US);

Inventors:

Sungbo Shim, Irvine, CA (US);

Kang N. Lee, Strongsville, OH (US);

Assignees:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 41/91 (2006.01); C04B 41/00 (2006.01); C04B 41/45 (2006.01); C04B 41/89 (2006.01); C04B 41/52 (2006.01); F01D 5/28 (2006.01); C04B 35/80 (2006.01); C04B 41/81 (2006.01);
U.S. Cl.
CPC ...
C04B 41/91 (2013.01); C04B 35/80 (2013.01); C04B 41/009 (2013.01); C04B 41/0072 (2013.01); C04B 41/459 (2013.01); C04B 41/52 (2013.01); C04B 41/81 (2013.01); C04B 41/89 (2013.01); F01D 5/288 (2013.01); C04B 2235/72 (2013.01); F05D 2300/2102 (2013.01); F05D 2300/6033 (2013.01);
Abstract

Example techniques may include depositing a slurry on at least a predetermined surface region of a ceramic matrix composite substrate. The slurry may include a solvent and particles comprising at least one of silicon metal or silicon carbide. The slurry may be dried to form a wicking layer on the predetermined surface region. The ceramic matrix composite substrate and the wicking layer may be heated to a temperature of at least 900° C. to wick at least one wickable species from the ceramic matrix composite substrate into the wicking layer. Substantially all of the wicking layer may be removed from the predetermined surface region. Example articles may include a ceramic matrix composite substrate. A wicking layer may be disposed on at least a predetermined surface region of the ceramic matrix composite substrate. The wicking layer may include at least one wicked species wicked from the ceramic matrix composite substrate.