The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 07, 2020

Filed:

Dec. 15, 2014
Applicant:

Panasonic Intellectual Property Management Co., Ltd., Osaka, JP;

Inventors:

Atsuhiro Kawamoto, Hyogo, JP;

Junji Fujiwara, Osaka, JP;

Yukinori Hirota, Hyogo, JP;

Noriyuki Matsuoka, Osaka, JP;

Kaito Matsui, Osaka, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B23K 9/095 (2006.01); B23K 9/23 (2006.01); B23K 9/173 (2006.01); B23K 9/09 (2006.01); B23K 9/073 (2006.01); B23K 9/12 (2006.01); B23K 103/04 (2006.01); B23K 101/34 (2006.01); B23K 101/18 (2006.01);
U.S. Cl.
CPC ...
B23K 9/095 (2013.01); B23K 9/073 (2013.01); B23K 9/0732 (2013.01); B23K 9/09 (2013.01); B23K 9/092 (2013.01); B23K 9/124 (2013.01); B23K 9/173 (2013.01); B23K 9/23 (2013.01); B23K 2101/18 (2018.08); B23K 2101/34 (2018.08); B23K 2103/04 (2018.08);
Abstract

As a conventional problem, welding on surface-treated material, such as a zinc-coated steel plate, considerably generates air holes including blowholes and also generates lots of spatters. Present invention provides a method of controlling arc welding performed in a manner that a short-circuit period, in which a short circuit is generated between a welding wire and an object to be welded, and an arc period, in which an arc is generated after release of the short circuit, are repeated alternately. According to the method, welding current is increased from an arc-regeneration-before current to a first welding current at a detection of release of the short circuit such that an increase gradient of the welding current becomes not less than 750 A/msec. This suppresses generation of air holes and spatters in welding work on a surface-treated material, such as a zinc-coated steel plate.