The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 24, 2020

Filed:

May. 16, 2017
Applicant:

Sumitomo Riko Company Limited, Komaki-shi, Aichi, JP;

Inventors:

Tomoyuki Fukuyasu, Komaki, JP;

Makoto Shimojo, Komaki, JP;

Atsuo Miyajima, Komaki, JP;

Kazuki Hatanaka, Komaki, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B29C 49/00 (2006.01); B29C 57/04 (2006.01); B60K 15/04 (2006.01); B60K 15/01 (2006.01); B29C 35/02 (2006.01); B29L 31/00 (2006.01); B29L 23/00 (2006.01);
U.S. Cl.
CPC ...
B29C 49/0015 (2013.01); B29C 35/02 (2013.01); B29C 57/04 (2013.01); B60K 15/01 (2013.01); B60K 15/04 (2013.01); B29K 2023/06 (2013.01); B29L 2023/22 (2013.01); B29L 2031/7172 (2013.01);
Abstract

A manufacturing process for filler tube includes: a workpiece arrangement step of arranging a workpiece onto an outer peripheral mold not only to axially lock a to-be-locked portion with respect to a locking portion but also so as to make the outer peripheral mold, which is set at a predetermined temperature, support a cylinder-shaped body of the workpiece on the outer peripheral face; and a flare-molding step of flare molding a flange by inserting an inner peripheral mold, which is set at a higher temperature than the predetermined temperature of the outer peripheral mold, into a to-be-molded portion on the inner peripheral side, and by relatively moving the outer peripheral mold and the inner peripheral mold in the axial direction to make a counter-welding-face forming portion and a welding-face forming portion clamp the to-be-molded portion between them in the axial direction.