The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 17, 2020

Filed:

Mar. 26, 2014
Applicant:

Kobe Steel, Ltd., Kobe-shi, JP;

Inventor:

Kei Masumoto, Kobe, JP;

Assignee:

Kobe Steel, Ltd., Kobe-shi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01F 1/147 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/20 (2006.01); C22C 38/34 (2006.01); C22C 38/42 (2006.01); C23C 8/10 (2006.01); C22C 38/60 (2006.01); C21D 8/12 (2006.01); C21D 1/26 (2006.01); C21D 6/00 (2006.01); C22C 38/08 (2006.01); C22C 38/16 (2006.01); H01F 41/00 (2006.01);
U.S. Cl.
CPC ...
H01F 1/14766 (2013.01); C21D 1/26 (2013.01); C21D 6/001 (2013.01); C21D 6/002 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/1272 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/004 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/16 (2013.01); C22C 38/20 (2013.01); C22C 38/34 (2013.01); C22C 38/42 (2013.01); C22C 38/60 (2013.01); C23C 8/10 (2013.01); H01F 1/147 (2013.01); H01F 41/00 (2013.01);
Abstract

The present invention inexpensively provides a steel material having greater corrosion resistance than electromagnetic stainless steel and also having excellent magnetic properties. The steel material comprises, in % by mass, 0.001%-0.025% C, 1.0%-4.0% Si, 0.1%-1.0% Mn, more than 0% but no more than 0.030% P, more than 0% but no more than 0.10% S, more than 0% but less than 4.0% Cr, more than 0% but no more than 0.010% Al, and more than 0% but no more than 0.01% N, with the remainder being iron and unavoidable impurities; and is characterized by having an oxide coating formed on the steel surface material, said oxide coating including either Si or Cr, or both, including a non-crystalline layer, and having a thickness of 50-500 nm.