The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 10, 2020

Filed:

Sep. 18, 2017
Applicant:

Nanjing University, Nanjing, CN;

Inventors:

Bingcai Pan, Nanjing, CN;

Xiaolin Zhang, Nanjing, CN;

Siyuan Pan, Nanjing, CN;

Cheng Cheng, Nanjing, CN;

Zefang Chen, Nanjing, CN;

Assignee:

NANJING UNIVERSITY, Nanjing, unknown;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B01J 20/26 (2006.01); B01J 20/28 (2006.01); C02F 1/28 (2006.01); B01J 41/14 (2006.01); B01J 20/02 (2006.01);
U.S. Cl.
CPC ...
B01J 20/265 (2013.01); B01J 20/0222 (2013.01); B01J 20/0229 (2013.01); B01J 20/0233 (2013.01); B01J 20/28007 (2013.01); B01J 20/28059 (2013.01); B01J 20/28061 (2013.01); B01J 41/14 (2013.01); C02F 1/288 (2013.01); C02F 1/285 (2013.01); C02F 2305/08 (2013.01);
Abstract

A resin nanocomposite, including a resin skeleton structure and nanoparticles. The resin skeleton structure is an aminated polystyrene. The nanoparticles are dispersed in the resin skeleton structure. The specific area of the nanocomposite is between 50 and 300 m/g, and the pore size thereof is between 5 and 40 nm. The invention also provides a method for preparing the resin nanocomposite, the method including: 1) mixing and dissolving a linear polyethylene with a chloromethyl polystyrene or a polyvinyl chloride to yield a polymer solution, and adding the nanoparticles to the polymer solution; 2) adding an alcohol solution to liquid nitrogen; adding the mixed solution dropwise to the liquid nitrogen to yield a mixture; allowing the mixture to stand; collecting, washing and drying resin beads to yield a composite material; and 3) adding the composite material to an amine solution for reaction, and washing and drying the resulting product.