The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 03, 2020

Filed:

Jan. 27, 2015
Applicant:

Riken Technos Corporation, Tokyo, JP;

Inventors:

Taketo Hashimoto, Tokyo, JP;

Nozomu Washio, Tokyo, JP;

Assignee:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B05D 7/00 (2006.01); B05D 3/06 (2006.01); B05D 1/26 (2006.01); C08J 7/12 (2006.01); C08J 3/24 (2006.01); C08J 7/04 (2020.01);
U.S. Cl.
CPC ...
B05D 7/544 (2013.01); B05D 1/26 (2013.01); B05D 1/265 (2013.01); B05D 3/067 (2013.01); B05D 7/546 (2013.01); C08J 3/243 (2013.01); C08J 3/244 (2013.01); C08J 7/042 (2013.01); C08J 7/123 (2013.01); B05D 2252/02 (2013.01); C08J 2333/24 (2013.01); C08J 2367/02 (2013.01);
Abstract

Embodiments of the invention provide a method for producing a multilayer coated film which involves obtaining a first layered body by forming, on a film substrate, a wet-coated film including a coating material (A) containing an active energy ray-curable resin which contains a first photopolymerization initiator and a second photopolymerization initiator, the reaction wavelengths of which differ from one another; and forming a pre-cured coated film including the coating material (A) in a dry-to-the-touch state by preliminarily curing the wet-coated film including the coating material (A), by irradiating the first layered body with active energy rays which include the reaction wavelength of the first photopolymerization initiator and do not include the reaction wavelength of the second photopolymerization initiator. The method further includes obtaining a second layered body by forming a wet-coated film including a coating material (B) on the pre-cured coated film including the coating material (A); and obtaining the multilayer coated film by fully curing the pre-cured coated film including the coating material (A) by irradiating the second layered body with active energy rays including the reaction wavelength of the second photopolymerization initiator.