The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 18, 2020

Filed:

Jun. 14, 2018
Applicant:

Skc Co., Ltd., Suwon-si, Gyeonggi-do, KR;

Inventors:

Kyu-Hun Kim, Seoul, KR;

Jewon Yeon, Suwon-si, KR;

Sung Jin Chung, Seoul, KR;

Heung Sik Kim, Seoul, KR;

Hyejin Kim, Suwon-si, KR;

Hak Soo Lee, Suwon-si, KR;

Assignee:

SKC CO., LTD., Suwon-si, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 17/10 (2006.01); B32B 37/18 (2006.01); C09J 159/00 (2006.01);
U.S. Cl.
CPC ...
B32B 17/10761 (2013.01); B32B 17/10036 (2013.01); B32B 17/10577 (2013.01); B32B 17/10688 (2013.01); B32B 17/10954 (2013.01); B32B 37/182 (2013.01); B32B 17/10596 (2013.01); B32B 17/10935 (2013.01); C09J 159/00 (2013.01);
Abstract

Embodiments relate to a resin film for laminated glass, laminated glass comprising the resin film, and a process for manufacturing the laminated glass. The resin film for laminated glass comprises a resin layer comprising a polyvinyl acetal resin and a contact surface in direct contact with glass, wherein the contact surface has an Rz roughness of 25 to 90 μm and a maximum static friction coefficient at 20° C. of 0.85 to 1.60, and the compressive elastic deformation index measured in the perpendicular direction from the contact surface at 35° C. is 40 to 310 μm/N.