The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 18, 2020

Filed:

Aug. 23, 2016
Applicant:

Nike, Inc., Beaverton, OR (US);

Inventor:

Clayton Chambers, Portland, OR (US);

Assignee:

NIKE, Inc., Beaverton, OR (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B29D 35/14 (2010.01); B29D 35/04 (2010.01); B29C 45/16 (2006.01); B29C 35/16 (2006.01); B29C 45/00 (2006.01); B29C 35/00 (2006.01); B29C 35/08 (2006.01); B29D 35/00 (2010.01); B29C 43/14 (2006.01); B29D 35/12 (2010.01); B29K 21/00 (2006.01); B29L 31/50 (2006.01);
U.S. Cl.
CPC ...
B29D 35/142 (2013.01); B29C 35/0805 (2013.01); B29C 35/16 (2013.01); B29C 43/14 (2013.01); B29C 43/145 (2013.01); B29C 45/0001 (2013.01); B29C 45/16 (2013.01); B29C 45/1657 (2013.01); B29C 45/1671 (2013.01); B29D 35/0009 (2013.01); B29D 35/04 (2013.01); B29D 35/122 (2013.01); B29C 2035/0811 (2013.01); B29C 2043/147 (2013.01); B29C 2045/1664 (2013.01); B29K 2021/006 (2013.01); B29K 2995/0021 (2013.01); B29L 2031/504 (2013.01);
Abstract

An article is molded from first and second thermosetting elastomer compositions each comprising free-radically curable elastomer and free radical initiator but different from one another. The first thermosetting elastomer composition is molded to fill a first area of a mold cavity at a first temperature at which the first free radical initiator has a half-life≤about 10 minutes or at which the first thermosetting elastomer composition has an increase in torque less than 10% of a total increase in torque at full cure. The second thermosetting elastomer composition is then inserted into the mold cavity, and the mold is heated to fully cure the article, for example a temperature at which each free radical initiator has a half-life≤about 1 minute, with the second composition filling a second area of the mold cavity before or during heating and curing.