The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 04, 2020

Filed:

Sep. 13, 2017
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Jean-Michel Mataigne, Senlis, FR;

Luc Diez, Metz, FR;

Assignee:

ARCELORMITTAL, Luxembourg, LU;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C23C 2/06 (2006.01); C23C 26/00 (2006.01); C23C 2/04 (2006.01); C23C 2/26 (2006.01); B32B 15/04 (2006.01); B32B 15/18 (2006.01); B32B 15/01 (2006.01); B32B 15/20 (2006.01); C23C 2/00 (2006.01); C23C 30/00 (2006.01);
U.S. Cl.
CPC ...
C23C 2/06 (2013.01); B32B 15/01 (2013.01); B32B 15/012 (2013.01); B32B 15/04 (2013.01); B32B 15/18 (2013.01); B32B 15/20 (2013.01); C23C 2/00 (2013.01); C23C 2/04 (2013.01); C23C 2/26 (2013.01); C23C 26/00 (2013.01); C23C 30/00 (2013.01); C23C 30/005 (2013.01); Y10T 428/1241 (2015.01); Y10T 428/12229 (2015.01); Y10T 428/12792 (2015.01); Y10T 428/12799 (2015.01); Y10T 428/12972 (2015.01); Y10T 428/12979 (2015.01); Y10T 428/12993 (2015.01);
Abstract

A process for manufacturing a coated metal strip having a metallic corrosion protection coating is provided. The process includes passing a metal strip through a molten metal bath comprising from 2 to 8 wt % aluminum, 0 to 5 wt % magnesium, up to 0.3 wt % additional elements, and a balance including zinc and inevitable impurities, to yield a molten metal coated metal strip, wiping the molten metal coated metal strip with a nozzle spraying a gas on either side of the molten metal coated metal strip and cooling the coating in a controlled manner until the coating has completely solidified, to obtain the coated metal strip. A temperature of the molten metal bath is from 350 to 700° C., and the cooling is conducted at a rate less than 15° C./s between a temperature on leaving a unit where the wiping occurs and a start of solidification of the coating, and then at a rate greater than or equal to 15° C./s between a start and an end of solidification of the coating.