The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 14, 2020

Filed:

Apr. 11, 2017
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Yoshimasa Funakawa, Fukuyama, JP;

Tetsuo Yamamoto, Bangkok, TH;

Hiroshi Uchomae, Kawasaki, JP;

Hiroshi Nakano, Kurashiki, JP;

Taro Kizu, Kawasaki, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C21D 8/02 (2006.01); C21D 8/04 (2006.01); C22C 38/00 (2006.01); C22C 38/14 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/60 (2006.01); C22C 38/08 (2006.01); C22C 38/10 (2006.01); C22C 38/12 (2006.01); C22C 38/16 (2006.01); C22C 38/22 (2006.01); C22C 38/28 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); C21D 8/0226 (2013.01); C21D 8/0247 (2013.01); C21D 8/0263 (2013.01); C21D 8/0415 (2013.01); C21D 8/0426 (2013.01); C21D 8/0463 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/10 (2013.01); C22C 38/105 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22C 38/22 (2013.01); C22C 38/28 (2013.01); C22C 38/60 (2013.01); C21D 2211/004 (2013.01); C21D 2211/005 (2013.01); Y10T 428/12799 (2015.01); Y10T 428/12972 (2015.01);
Abstract

A method of manufacturing a high-strength hot rolled steel sheet by hot rolling a steel having a chemical composition including, by mass %: C: more than 0.010% and not more than 0.06%, Si: not more than 0.3%, Mn: not more than 0.8%, P: not more than 0.03%, S: not more than 0.02%, Al: not more than 0.1%, N: not more than 0.01% and Ti: 0.05 to 0.10%, the balance including Fe and inevitable impurities, including: after the steel is heated to an austenite single phase region, the steel is finish rolled at a finishing delivery temperature of 860° C. to 1050° C., the steel sheet is cooled at an average cooling rate of not less than 30° C./s in a temperature range of from a temperature after the completion of the finish rolling to 750° C., and the steel sheet is coiled into a coil at a coiling temperature of 580° C. to 700° C.