The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 07, 2020

Filed:

Jun. 01, 2015
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Tomoyuki Okubo, Kurashiki, JP;

Tadashi Nakanishi, Kurashiki, JP;

Yoshihiko Oda, Kurashiki, JP;

Shinji Koseki, Kawasaki, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C21D 9/00 (2006.01); C21D 8/12 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/60 (2006.01); C21D 1/30 (2006.01); H02K 1/02 (2006.01); H02K 15/02 (2006.01);
U.S. Cl.
CPC ...
C21D 9/0068 (2013.01); C21D 1/30 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); C21D 8/1261 (2013.01); C21D 8/1266 (2013.01); C21D 9/46 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/60 (2013.01); H02K 1/02 (2013.01); H02K 15/02 (2013.01);
Abstract

A non-oriented electrical steel sheet is obtained by subjecting a slab containing C: not more than 0.005 mass %, Si: 1.0-5.0 mass %, Mn: 0.04-3.0 mass %, sol. Al: not more than 0.005 mass %, P: 0.03-0.2 mass %, S: not more than 0.005 mass %, N: not more than 0.005 mass %, B: not more than 0.001 mass %, and Se: not more than 0.001 mass % and satisfying sol. Al+C+5B+5Se≤0.005 mass % to hot rolling, cold rolling and finish annealing. A sheet temperature at the outlet side of the rolling machine in at least one pass of the final cold rolling is set to a range of 100-300° C. to provide S/2M of not less than 1.0 and S/5C of not less than 1.0 when X-ray intensity ratios of {001}<250>, {111}<112> and {001}<100> in a central layer in a thickness direction are S, M and C, respectively.