The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 24, 2019

Filed:

Jul. 13, 2018
Applicant:

Sumitomo Metal Mining Co., Ltd., Tokyo, JP;

Inventors:

Tomoko Nakayama, Ehime, JP;

Rei Kokado, Ehime, JP;

Kensaku Mori, Ehime, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01B 1/08 (2006.01); H01M 4/485 (2010.01); H01M 4/525 (2010.01); C01G 53/00 (2006.01); H01M 10/0525 (2010.01); H01M 4/505 (2010.01); H01M 10/052 (2010.01);
U.S. Cl.
CPC ...
H01M 4/485 (2013.01); C01G 53/42 (2013.01); H01B 1/08 (2013.01); H01M 4/525 (2013.01); H01M 10/0525 (2013.01); C01P 2002/30 (2013.01); C01P 2002/76 (2013.01); C01P 2006/12 (2013.01); H01M 4/505 (2013.01); H01M 10/052 (2013.01); H01M 2220/20 (2013.01); H01M 2220/30 (2013.01);
Abstract

The purpose of the present invention is to easily provide at low cost, a cathode active material for non-aqueous electrolyte secondary batteries, which exhibits high particle strength and high weather resistance, while enabling achievement of excellent charge and discharge capacity and excellent output characteristics in cases where the cathode active material is used as a cathode material of a non-aqueous electrolyte secondary battery. A slurry of from 500 g/L to 2000 g/L is formed by adding water to a powder of a lithium nickel composite oxide represented by the general formula (A): LiNiCoMO, where 0.10≤x≤0.20, 0≤y≤0.10, 0.97≤z≤1.20, and M represents at least one element selected from among Mn, V, Mg, Mo, Nb, Ti and Al); the slurry is washed with water by stirring; and after filtration, the resulting material is subjected to a heat treatment at a temperature of from 120° C. to 550° C. (inclusive) in an oxygen atmosphere having an oxygen concentration of 80% by volume or more.