The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 17, 2019

Filed:

Dec. 08, 2016
Applicant:

Lg Chem, Ltd., Seoul, KR;

Inventors:

Sang Eun Park, Daejeon, KR;

Hae Woong Park, Daejeon, KR;

Choong Hoon Lee, Daejeon, KR;

Seung Hwan Jung, Daejeon, KR;

Ji Yoon Woo, Daejeon, KR;

Hyo Ju Kim, Daejeon, KR;

Young Woo Lee, Daejeon, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 210/16 (2006.01); C08F 2/04 (2006.01); C08F 4/42 (2006.01); C08F 210/02 (2006.01); C08F 210/06 (2006.01); C08F 210/08 (2006.01); C08F 210/14 (2006.01); C08F 212/08 (2006.01); C08F 212/36 (2006.01); C08F 236/06 (2006.01); C08F 236/04 (2006.01);
U.S. Cl.
CPC ...
C08F 210/16 (2013.01); C08F 2/04 (2013.01); C08F 4/42 (2013.01); C08F 210/02 (2013.01); C08F 210/06 (2013.01); C08F 210/08 (2013.01); C08F 210/14 (2013.01); C08F 212/08 (2013.01); C08F 212/36 (2013.01); C08F 236/045 (2013.01); C08F 236/06 (2013.01); C08F 2500/01 (2013.01); C08F 2500/04 (2013.01); C08F 2500/08 (2013.01); C08F 2800/20 (2013.01);
Abstract

The present invention provides an olefin-based polymer which satisfies the following conditions of (1) to (4) and is capable of exhibiting improved impact strength without degrading mechanical properties such as tensile strength: (1) density (d): from 0.850 to 0.910 g/cc, (2) melting index (MI, 190° C., 2.16 kg load conditions): from 0.1 to 100 g/10 min, (3) molecular weight distribution (MWD): from 1.5 to 3.0, and (4) two peaks are shown in a temperature range of −20° C. to 120° C. when taking measurements of temperature rising elution fractionation (TREF), and a relation of T(90)−T(50)≥60° C. is satisfied (where T(90) is a temperature at which 90 wt % of the olefin-based polymer is eluted, and T(50) is a temperature at which 50 wt % of the olefin-based polymer is eluted).