The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 17, 2019

Filed:

Apr. 13, 2017
Applicant:

Mtu Aero Engines Ag, Munich, DE;

Inventors:

Johannes Casper, Munich, DE;

Georg Schlick, Munich, DE;

Alexander Ladewig, Bad Wiessee, DE;

Assignee:

MTU Aero Engines AG, Munich, DE;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B22F 3/105 (2006.01); B22F 3/10 (2006.01); B33Y 10/00 (2015.01); B33Y 30/00 (2015.01); B23K 26/342 (2014.01); B23K 26/346 (2014.01); B23K 13/01 (2006.01); B22F 5/00 (2006.01);
U.S. Cl.
CPC ...
B22F 3/1017 (2013.01); B22F 3/1055 (2013.01); B22F 5/009 (2013.01); B23K 13/01 (2013.01); B23K 26/342 (2015.10); B23K 26/346 (2015.10); B33Y 10/00 (2014.12); B33Y 30/00 (2014.12); B22F 2003/1056 (2013.01); B22F 2999/00 (2013.01); Y02P 10/295 (2015.11);
Abstract

A method for manufacturing at least a metallic portion of a component: a) depositing metallic material layer by layer onto at least one building platform; b) locally fusing and/or sintering the material layer by layer by supplying energy by at least one high-energy beam in the region of a buildup and joining zone to form at least a portion of at least one component layer of the component portion and/or of the component; c) lowering the building platform layer by layer by a predefined layer thickness; and d) repeating the steps a) through c) until completion of the component portion and/or of the component. Before, during and/or after process step b), at least one further portion of the component layer is formed by locally fusing and/or sintering the material by inductive heating at a temperature or in a temperature range above the solidus temperature of the metallic material used. A system for manufacturing at least a portion of a component is also provided.