The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 03, 2019

Filed:

Jan. 14, 2015
Applicant:

Baoshan Iron & Steel Co., Ltd., Shanghai, CN;

Inventors:

Guoli Zhai, Shanghai, CN;

Qingchao Tian, Shanghai, CN;

Qijiang Wang, Shanghai, CN;

Cailing Liu, Shanghai, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/10 (2006.01); C22C 38/48 (2006.01); C22C 38/58 (2006.01); C21D 9/08 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/04 (2006.01); C22C 38/20 (2006.01); C22C 38/22 (2006.01); C22C 38/24 (2006.01); C22C 38/26 (2006.01); C22C 38/32 (2006.01); C22C 38/38 (2006.01);
U.S. Cl.
CPC ...
C21D 8/105 (2013.01); C21D 9/08 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/20 (2013.01); C22C 38/22 (2013.01); C22C 38/24 (2013.01); C22C 38/26 (2013.01); C22C 38/32 (2013.01); C22C 38/38 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/48 (2013.01); C22C 38/58 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01);
Abstract

A high strength and toughness seamless steel tube for an automobile airbag, comprising the following elements, by wt %: C: 0.05-0.15%; Si: 0.1-0.45%; Mn: 1.0-1.9%; Ni: 0.1-0.6%; Cr: 0.05-1.0%; Mo: 0.05-0.2%; Cu: 0.05-0.50%; Al: 0.015-0.060%; Nb: 0.02-0.1%; V: 0.02-0.15%; and the balance being Fe and other inevitable impurities. A method for manufacturing the seamless steel tube comprises the steps: (1) heating a tube blank and then soaking; (2) hot piercing, reducing the diameter and the wall thickness of the tube blank with a stretch reducer and then cooling naturally; (3) annealing, pickling, phosphating and saponifying; (4) cold working to obtain a finished product size; and (5) carrying out stress relief annealing treatment.


Find Patent Forward Citations

Loading…