The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 12, 2019

Filed:

Nov. 12, 2015
Applicant:

Nippon Steel Chemical & Material Co., Ltd., Tokyo, JP;

Inventors:

Noriko Yamada, Tokyo, JP;

Sawako Yamaguchi, Tokyo, JP;

Koichi Nose, Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C09D 183/04 (2006.01); C23C 14/34 (2006.01); C23C 14/16 (2006.01); C09D 7/00 (2018.01); C08G 77/00 (2006.01); C09D 7/40 (2018.01); B05D 7/14 (2006.01); B05D 7/24 (2006.01); B32B 15/08 (2006.01); C09D 7/20 (2018.01); C09D 7/63 (2018.01); C08G 77/08 (2006.01);
U.S. Cl.
CPC ...
C09D 183/04 (2013.01); B05D 7/14 (2013.01); B05D 7/24 (2013.01); B32B 15/08 (2013.01); C08G 77/08 (2013.01); C09D 7/20 (2018.01); C09D 7/40 (2018.01); C09D 7/63 (2018.01); C23C 14/165 (2013.01); C23C 14/3407 (2013.01); C08G 77/80 (2013.01);
Abstract

Problems to be Solved: To provide a metal foil coil with a planarization film, with which an electronic device can be formed by a roll to roll process. Solution: A quick curable coating liquid for a planarization film prepared by adding into an organic solvent, with respect to 1 mol of a phenyltrialkoxysilane, 0.1 mol to 1 mol of acetic acid and 0.005 mol to 0.05 mol of organic tin as a catalyst, hydrolyzing the silane with 2 mol to 4 mol of water, then distilling away the organic solvent at a temperature of 160° C. to 210° C. under reduced pressure to yield a resin, and dissolving the resin in an aromatic hydrocarbon solvent, is coated on a metal foil coil to a film thickness of 2.0 μm to 5.0 μm. When an insulation coating is provided on a metal foil coil before a planarization film is formed, high reliability for insulation can be obtained. When a stainless steel foil provided with a reflection film is used, a highly efficient light emitting device can be obtained.


Find Patent Forward Citations