The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 12, 2019

Filed:

Mar. 31, 2016
Applicant:

Easyl, Bonneville, FR;

Inventors:

Francois Lacoste, Neuilly sur Seine, FR;

Julien Thiel, Arbusigny, FR;

Assignee:

EASYL, Bonneville, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C01G 9/00 (2006.01); C01F 11/00 (2006.01); B01D 9/00 (2006.01); A01N 59/16 (2006.01); B01J 23/06 (2006.01); H01M 4/08 (2006.01); H01M 4/24 (2006.01); H01M 4/26 (2006.01); H01M 4/58 (2010.01); H01M 4/62 (2006.01); B01J 37/04 (2006.01); B01J 37/08 (2006.01); B01J 35/00 (2006.01); B01J 37/00 (2006.01); B02C 17/16 (2006.01); B02C 17/18 (2006.01);
U.S. Cl.
CPC ...
C01G 9/00 (2013.01); A01N 59/16 (2013.01); B01D 9/0063 (2013.01); B01J 23/06 (2013.01); B01J 35/002 (2013.01); B01J 37/0036 (2013.01); B01J 37/04 (2013.01); B01J 37/08 (2013.01); B02C 17/163 (2013.01); B02C 17/183 (2013.01); C01F 11/00 (2013.01); H01M 4/08 (2013.01); H01M 4/244 (2013.01); H01M 4/26 (2013.01); H01M 4/5825 (2013.01); H01M 4/62 (2013.01); B01D 2009/0086 (2013.01); C01P 2002/72 (2013.01); C01P 2004/03 (2013.01); C01P 2004/51 (2013.01); C01P 2004/61 (2013.01); C01P 2006/10 (2013.01);
Abstract

Disclosed is a method for manufacturing calcium zincate crystals including: placing calcium hydroxideand zinc oxide, one of the precursors thereof, or one of the water mixtures thereof in a starting suspension, the mass ratio of water to calcium hydroxide and zinc oxide, or one of the precursors or mixtures thereof, being greater than or equal to 1; milling the starting suspension to an ambient temperature less than or equal to 50° C. in a wet-phase three-dimensional micro-ball mill for a residence time less than or equal to 15 minutes and in particular from 5 to 25 seconds; recovering a calcium zincate crystal suspension coming out of the mill; and optionally, concentrating or drying the calcium zincate crystal suspension so as to obtain a calcium zincate crystal powder. Also disclosed are uses associated with the calcium zincate crystals obtained according to the method described above.