The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 12, 2019

Filed:

Jul. 12, 2016
Applicant:

R.j. Reynolds Tobacco Products, Winston-Salem, NC (US);

Inventors:

Andries Don Sebastian, Clemmons, NC (US);

Sami Ilmari Sneck, Espoo, FI;

Mikko Juhani Söderlund, Helsinki, FI;

Assignee:

R.J. REYNOLDS TOBACCO PRODUCTS, Winston-Salem, NC (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
A24F 15/00 (2006.01); B65D 85/10 (2006.01); B65D 85/12 (2006.01); B65D 65/02 (2006.01); B65D 65/40 (2006.01); C23C 16/06 (2006.01); C23C 16/455 (2006.01); B65D 25/36 (2006.01); C23C 16/40 (2006.01);
U.S. Cl.
CPC ...
B65D 65/02 (2013.01); A24F 15/00 (2013.01); B65D 25/36 (2013.01); B65D 65/40 (2013.01); B65D 85/1045 (2013.01); C23C 16/06 (2013.01); C23C 16/40 (2013.01); C23C 16/403 (2013.01); C23C 16/405 (2013.01); C23C 16/45525 (2013.01); C23C 16/45555 (2013.01); Y02W 90/12 (2015.05); Y02W 90/13 (2015.05);
Abstract

Provided herein is a moisture barrier film for packaging, such as tobacco or cigarette packaging. The film comprises polylactic acid ('PLA') that is both biodegradable and transparent. The film includes multiple layers of PLA, with a base layer having a relatively high melting point compared to two outer layers, which have a relatively low melting point. The outer layers provide heat sealing capabilities to the film. The film is coated with a metal oxide layer comprised of aluminum oxide, titanium oxide, and/or aluminum-titanium oxide using an atomic layer deposition ('ALD') coating method. The ALD coating to the PLA film results in a moisture transmission rate of less than 4 g/m2/day after the film has been subjected to creasing, which induces cracking of the ALD metal oxide layer.


Find Patent Forward Citations

Loading…