The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 29, 2019

Filed:

Nov. 17, 2015
Applicant:

Jfe Steel Corporation, Chiyoda-ku, Tokyo, JP;

Inventors:

Kunio Fukuda, Tokyo, JP;

Shin Ishikawa, Tokyo, JP;

Mitsuyuki Fujisawa, Tokyo, JP;

Katsuhisa Yamauchi, Tokyo, JP;

Chikara Kami, Tokyo, JP;

Assignee:

JFE STEEL CORPORATION, Chiyoda-ku, Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C23C 8/26 (2006.01); C22C 38/42 (2006.01); C22C 38/02 (2006.01); C21D 1/76 (2006.01); C22C 38/00 (2006.01); C21D 9/46 (2006.01); C22C 38/48 (2006.01); C22C 38/04 (2006.01); C21D 1/06 (2006.01); C22C 38/54 (2006.01); C22C 38/06 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/50 (2006.01);
U.S. Cl.
CPC ...
C23C 8/26 (2013.01); C21D 1/06 (2013.01); C21D 1/76 (2013.01); C21D 9/46 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/54 (2013.01);
Abstract

Provided is a ferritic stainless steel having a chemical composition containing, in mass %: 0.003% to 0.025% of C; 0.05% to 1.00% of Si; 0.05% to 1.00% of Mn; 0.04% or less of P; 0.01% or less of S; 16.0% to 23.0% of Cr; 0.20% to 0.80% of Cu; 0.05% to 0.60% of Ni; 0.20% to 0.70% of Nb; 0.005% to 0.020% of N; and the balance being Fe and incidental impurities, in which a nitrogen-enriched layer is present that has a nitrogen concentration peak value of 0.03 mass % to 0.30 mass % at a depth of within 0.05 μm of a surface of the steel.