The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 22, 2019

Filed:

Jul. 24, 2013
Applicant:

Thyssenkrupp Steel Europe Ag, Duisburg, DE;

Inventors:

Rainer Fechte-Heinen, Bottrop, DE;

Christian Höckling, Mülheim an der Ruhr, DE;

Lothar Patberg, Moers, DE;

Jens-Ulrik Becker, Duisburg, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); B22D 11/06 (2006.01); B22D 11/12 (2006.01); C22F 1/00 (2006.01); C22C 38/00 (2006.01); C22C 38/34 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01); C22C 38/52 (2006.01); C22C 38/58 (2006.01); B21B 1/46 (2006.01); B22D 11/00 (2006.01); B22D 11/041 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/42 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B21B 1/46 (2013.01); B22D 11/001 (2013.01); B22D 11/041 (2013.01); B22D 11/0622 (2013.01); B22D 11/1206 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/007 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/34 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/52 (2013.01); C22C 38/58 (2013.01); C22F 1/006 (2013.01); B21B 1/463 (2013.01);
Abstract

Methods for producing a flat product from an iron-based shape memory alloy may involve casting a melt comprised of iron, alloying elements, and impurities into a strip having a thickness of 1-30 mm and cooling the melt as the strip is formed. A twin-roll caster may be employed to help cool and form the melt into the strip. The resultant flat product is highly resistant to bending and is robust under pressure and torsion.


Find Patent Forward Citations

Loading…