The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 15, 2019

Filed:

May. 22, 2017
Applicant:

Fujifilm Corporation, Tokyo, JP;

Inventor:

Satoshi Wakamatsu, Kanagawa, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
A61M 37/00 (2006.01); A61K 9/00 (2006.01); B29C 39/24 (2006.01); A61K 47/36 (2006.01); A61K 47/38 (2006.01); B29D 7/01 (2006.01); B29L 31/00 (2006.01); A61K 9/70 (2006.01);
U.S. Cl.
CPC ...
A61K 9/0021 (2013.01); A61K 47/36 (2013.01); A61K 47/38 (2013.01); A61M 37/0015 (2013.01); B29C 39/24 (2013.01); A61K 9/7007 (2013.01); A61M 2037/0053 (2013.01); B29D 7/01 (2013.01); B29L 2031/7544 (2013.01);
Abstract

A method of producing a transdermal absorption sheet includes: filling needle-like recessed portions on a mold having the needle-like recessed portions with a polymer solution; drying the filled polymer solution to form a polymer layer; and peeling off the polymer layer, wherein, in drying the polymer solution, low rate drying conditions are set in a concentration range in which an average solid content concentration of the polymer solution is 70 wt % to 80 wt %. When a constant drying rate of water is used as an index, in the concentration range in which the average solid content concentration of the polymer solution is 70 wt % to 80 wt %, and the constant drying rate is lower than a maximum value of a constant drying rate under a drying condition where the average solid content concentration of the polymer solution is less than 70 wt % and more than 80 wt %.