The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 01, 2019

Filed:

Feb. 27, 2013
Applicant:

Jfe Steel Corporation, Chiyoda-ku, Tokyo, JP;

Inventors:

Masanori Uesaka, Tokyo, JP;

Minoru Takashima, Tokyo, JP;

Takeshi Imamura, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01F 1/147 (2006.01); C21D 9/46 (2006.01); C21D 1/26 (2006.01); C22C 38/60 (2006.01); H01F 1/16 (2006.01); C21D 8/12 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/16 (2006.01); C22C 38/34 (2006.01); H01F 41/02 (2006.01);
U.S. Cl.
CPC ...
H01F 1/14775 (2013.01); C21D 1/26 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); C21D 8/1261 (2013.01); C21D 8/1272 (2013.01); C21D 9/46 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/16 (2013.01); C22C 38/34 (2013.01); C22C 38/60 (2013.01); H01F 1/16 (2013.01); H01F 41/02 (2013.01);
Abstract

In a method for producing a grain-oriented electrical steel sheet by hot rolling a steel slab comprising C: 0.04-0.12 mass %, Si: 1.5-5.0 mass %, Mn: 0.01-1.0 mass %, sol. Al: 0.010-0.040 mass %, N: 0.004-0.02 mass %, one or two of S and Se: 0.005-0.05 mass % in total of S and Se, cold rolling, and subjecting to primary recrystallization annealing and further to final annealing, a content ratio of sol. Al to N in the steel slab (sol. Al/N) and a final thickness d (mm) satisfy an equation of 4d+1.52≤sol. Al/N≤4d+2.32, and the steel sheet in the heating process of the final annealing is held at a temperature of 775-875° C. for 40-200 hours and then heated in a temperature region of 875-1050° C. at a heating rate of 10-60° C./hr to preform secondary recrystallization and purification treatment, whereby an extremely-thin grain-oriented electrical steel sheet having a low iron loss and a small deviation in coil is produced.