The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 17, 2019

Filed:

Nov. 08, 2012
Applicants:

Changchun Hipolyking Co., Ltd, ChangChun, CN;

Mengxian Ding, Changchun, CN;

Inventors:

Xin Zhang, Jilin, CN;

Jibin Zhong, Jilin, CN;

Mengxian Ding, ChangChun, CN;

Xiaoyi Lv, Jilin, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08G 73/10 (2006.01); C08L 79/08 (2006.01);
U.S. Cl.
CPC ...
C08G 73/1032 (2013.01); C08G 73/105 (2013.01); C08G 73/1014 (2013.01); C08G 73/1046 (2013.01); C08G 73/1053 (2013.01); C08G 73/1067 (2013.01); C08G 73/1071 (2013.01); C08L 79/08 (2013.01);
Abstract

The present invention provides a preparation method of polyimide, comprising the following steps: a) carrying out a dehydration polymerization reaction on a diamine and an anhydride of an organic acid in a non-polar solvent to obtain a mixture, the non-polar solvent being one or more of arene, aliphatic hydrocarbon, halogenated arene and halogenated aliphatic hydrocarbon, and the anhydride of the organic acid being one or more of dianhydride and single anhydride: and b) filtering the mixture obtained in step a) and drying to obtain the polyimide. In the present invention, the dehydration polymerization reaction between the diamine and the anhydride of the organic acid can be carried out directly in the non-polar solvent to obtain the polyimide which cannot be dissolved in the non-polar solvent. Therefore, polyimide powder with fine particles can be obtained by directly filtering and drying the reaction mixture without washing. Not only complex washing and grinding processes are not needed, but also the production period is shortened, the production cost is reduced, and the large-scale production becomes more convenient.