The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 10, 2019

Filed:

Oct. 25, 2016
Applicant:

Jiangsu Hengli Chemical Fibre Co., Ltd., Suzhou, CN;

Inventors:

Guanfan Jin, Suzhou, CN;

Yiwei Shao, Suzhou, CN;

Ye Zhang, Suzhou, CN;

Lijun Wang, Suzhou, CN;

Huaizhi Zhuo, Suzhou, CN;

Zhujun Ding, Suzhou, CN;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C08G 63/183 (2006.01); C08G 63/86 (2006.01); D01F 1/10 (2006.01); D01F 6/92 (2006.01); C08G 63/83 (2006.01); D02G 1/18 (2006.01); D01F 6/62 (2006.01); C25B 3/12 (2006.01); D01D 5/08 (2006.01); D06P 1/16 (2006.01);
U.S. Cl.
CPC ...
C08G 63/183 (2013.01); C08G 63/83 (2013.01); C08G 63/86 (2013.01); C08G 63/866 (2013.01); C25B 3/12 (2013.01); D01F 1/10 (2013.01); D01F 6/62 (2013.01); D01F 6/92 (2013.01); D02G 1/18 (2013.01); D01D 5/08 (2013.01); D06P 1/16 (2013.01);
Abstract

A low chromatic aberration polyester different-shrinkage composite yarn is made of polyester POY yarn and polyester FDY composite yarn. The polyester POY yarn and polyester FDY yarn is obtained by spinning the polyester solution, the rupture strength of the low color polyester different-shrinkage composite yarn is ≥1.9 cN/dtex, the elongation at break is 30.0±5.0%, the crimp shrinkage is 2.50±3.0%, the network degree is 20±5/m, the color difference ΔE is less than 0.200. In the invention, the magnesium ethylene glycol is relatively mild, the thermal degradation coefficient is small, the oligomers in the polymerization process is reduced, and the oligomers in the dissolution process are further reduced, so that the appearance of stains and streaks reduces during the dyeing and post-processing heat setting of the polyester fiber, which ensures the fiber's leveling and rubbing fastness.