The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 20, 2019

Filed:

Aug. 29, 2017
Applicant:

Citic Dicastal Co., Ltd., Qinhuangdao, Hebei, CN;

Inventors:

Haiping Chang, Qinhuangdao, CN;

Zhixue Wang, Qinhuangdao, CN;

Shiyou Gao, Qinhuangdao, CN;

Jin Zhang, Qinhuangdao, CN;

Rui Li, Qinhuangdao, CN;

Dawei Xu, Qinhuangdao, CN;

Donghui Zhang, Qinhuangdao, CN;

Assignee:

CITIC Dicastal CO., LTD., Qinhuangdao, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 26/352 (2014.01); B23K 26/34 (2014.01); C23C 24/10 (2006.01); C23C 4/04 (2006.01); C23C 16/48 (2006.01);
U.S. Cl.
CPC ...
B23K 26/352 (2015.10); B23K 26/34 (2013.01); C23C 24/103 (2013.01); C23C 4/04 (2013.01); C23C 16/483 (2013.01);
Abstract

A spinning roller surface laser reinforced processing forming method is provided. A spinning roller is normalized after forging, the normalizing temperature is controlled to 860-880 DEG C., and the heat preservation time is 40-60 minutes; the spinning roller forging blank is roughly processed to reserve a tolerance allowance of 0.5 mm on the designated working face; the spinning roller and workpiece contact surface reinforcing layer is made of Ni625+WC2, in which WC is more than 22%; a reinforcing layer having the thickness of 0.8 mm is clad with laser on the working face of the spinning roller, and the preheating temperature is controlled to 250-400 DEG C. before welding; the spinning roller laser clad reinforcing layer is rolled; and the rolled spinning roller is put into a thermal treatment furnace for thermal treatment, and quenching and tempering treatment, re-crystallization and residual stress elimination are performed.