The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 13, 2019

Filed:

Jun. 05, 2017
Applicant:

Huazhong University of Science and Technology, Wuhan, CN;

Inventors:

Chunze Yan, Wuhan, CN;

Yusheng Shi, Wuhan, CN;

Wei Zhu, Wuhan, CN;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C23F 4/04 (2006.01); B33Y 10/00 (2015.01); C01B 32/186 (2017.01); C01B 32/184 (2017.01); C01B 32/194 (2017.01);
U.S. Cl.
CPC ...
C23F 4/04 (2013.01); B33Y 10/00 (2014.12); C01B 32/184 (2017.08); C01B 32/186 (2017.08); C01B 32/194 (2017.08); C01B 2204/32 (2013.01); C01P 2006/12 (2013.01); C01P 2006/14 (2013.01); C01P 2006/16 (2013.01);
Abstract

A method for preparing a three-dimensional porous graphene material, including: a) constructing a CAD model corresponding to a required three-dimensional porous structure, and designing an external shape and internal structure parameters of the model; b) based on the CAD model, preparing a three-dimensional porous metal structure using a metal powder as material; c) heating the three-dimensional porous metal structure and preparing a metal template of the required three-dimensional porous structure; d) placing the metal template in a tube furnace and heating the metal template to a temperature of between 800 and 1000° C.; standing for 0.5-1 hr, introducing a carbon source to the tube furnace for continued reaction, cooling resulting products to room temperature to yield a three-dimensional graphene grown on the metal template; and e) preparing a corrosive solution, and immersing the three-dimensional graphene in the corrosive solution.