The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 13, 2019

Filed:

Nov. 23, 2016
Applicant:

Teijin Film Solutions Limited, Tokyo, JP;

Inventors:

Naoki Iyo, Tokyo, JP;

Mitsuo Tojo, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/09 (2006.01); B32B 27/36 (2006.01); B32B 7/04 (2019.01); B32B 15/18 (2006.01); B32B 15/20 (2006.01); B32B 27/08 (2006.01); B32B 27/20 (2006.01); B32B 1/02 (2006.01);
U.S. Cl.
CPC ...
B32B 15/09 (2013.01); B32B 1/02 (2013.01); B32B 7/04 (2013.01); B32B 15/18 (2013.01); B32B 15/20 (2013.01); B32B 27/08 (2013.01); B32B 27/20 (2013.01); B32B 27/36 (2013.01); B32B 2250/04 (2013.01); B32B 2264/102 (2013.01); B32B 2264/104 (2013.01); B32B 2270/00 (2013.01); B32B 2307/306 (2013.01); B32B 2307/40 (2013.01); B32B 2307/402 (2013.01); B32B 2307/4026 (2013.01); B32B 2307/422 (2013.01); B32B 2307/518 (2013.01); B32B 2307/538 (2013.01); B32B 2307/584 (2013.01); B32B 2307/70 (2013.01); B32B 2307/704 (2013.01); B32B 2307/732 (2013.01); B32B 2367/00 (2013.01); B32B 2439/66 (2013.01); Y10T 428/24355 (2015.01);
Abstract

A colored biaxially stretched polyester film for metal plate attachment and forming processing, includes three layers: opposite surface layers (layers A) that contain substantially no coloring pigment and are made of a copolyester having an intrinsic viscosity of 0.65 to 0.80 and a melting point (TmA) of 230 to 260° C.; and a core layer (layer B) that has a coloring pigment content of more than 10 wt % and 50 wt % or less and is made of a copolyester having an intrinsic viscosity of 0.55 to 0.70 and a melting point (TmB) of 230 to 260° C. The film has a surface roughness within a range of 10 to 40 nm, and (TmB−TmA) is 4° C. or less.