The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 23, 2019

Filed:

Nov. 23, 2015
Applicant:

Saint-gobain Glass France, Courbevoie, FR;

Inventors:

Young Seong Lee, Seoul, KR;

Jin Woo Han, Seoul, KR;

Assignee:

SAINT-GOBAIN GLASS FRANCE, Courbevoie, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/04 (2006.01); B32B 17/06 (2006.01); H01L 51/52 (2006.01); C03C 8/04 (2006.01); C03C 17/00 (2006.01); C03C 17/04 (2006.01); C03C 17/34 (2006.01); C03C 21/00 (2006.01); H01L 51/00 (2006.01); H01L 51/56 (2006.01); C09D 1/00 (2006.01); B05D 1/26 (2006.01); B05D 3/02 (2006.01); C23C 30/00 (2006.01); C09D 7/61 (2018.01);
U.S. Cl.
CPC ...
H01L 51/5268 (2013.01); B05D 1/265 (2013.01); B05D 3/0254 (2013.01); C03C 8/04 (2013.01); C03C 17/007 (2013.01); C03C 17/04 (2013.01); C03C 17/3417 (2013.01); C03C 21/008 (2013.01); C09D 1/00 (2013.01); C09D 7/61 (2018.01); C23C 30/00 (2013.01); H01L 51/0021 (2013.01); H01L 51/0096 (2013.01); H01L 51/5206 (2013.01); H01L 51/56 (2013.01); C03C 2217/228 (2013.01); C03C 2217/425 (2013.01); C03C 2217/452 (2013.01); C03C 2217/91 (2013.01); C03C 2217/948 (2013.01); H01L 2251/303 (2013.01); H01L 2251/308 (2013.01); H01L 2251/556 (2013.01); H01L 2251/558 (2013.01); Y02E 10/549 (2013.01);
Abstract

A method for preparing a laminate substrate for a light emitting device includes providing a glass substrate having a refraction index, at 550 nm, of between 1.45 and 1.65, coating a glass frit having a refractive index, at 550 nm, of at least 1.7 onto the glass substrate, firing the resulting frit coated glass substrate at a temperature above the Littleton temperature of the glass frit thereby forming a first high index enamel layer, coating a metal oxide layer onto the first high index enamel layer, and firing the resulting coated glass substrate at a temperature above the Littleton temperature of the glass frit, thereby making react the metal oxide with the underlying first high index enamel layer and forming a second high index enamel layer with a plurality of spherical voids embedded in the upper section of the second high index enamel layer near the interface with air.