The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 02, 2019

Filed:

Aug. 01, 2012
Applicants:

Nobusuke Kariya, Fukuyama, JP;

Shinjiro Kaneko, Chiba, JP;

Yasunobu Nagataki, Chiyoda-ku, JP;

Inventors:

Nobusuke Kariya, Fukuyama, JP;

Shinjiro Kaneko, Chiba, JP;

Yasunobu Nagataki, Chiyoda-ku, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B32B 15/01 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C21D 8/02 (2006.01); C23C 2/06 (2006.01); C23C 2/02 (2006.01); C22C 18/00 (2006.01); C22C 18/04 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/16 (2006.01); C22C 38/18 (2006.01);
U.S. Cl.
CPC ...
C23C 2/02 (2013.01); B32B 15/013 (2013.01); C21D 8/0273 (2013.01); C22C 18/00 (2013.01); C22C 18/04 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22C 38/18 (2013.01); C23C 2/06 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/009 (2013.01); Y10T 428/12799 (2015.01);
Abstract

Provided are a high-strength hot-dip galvanized steel sheet having excellent formability and a tensile strength of 440 MPa or more and a method for manufacturing the same. A steel sheet has a microstructure containing a ferrite phase having an area fraction of 60% or more, a pearlite phase having an area fraction of 20% to 30%, and a bainite phase having an area fraction of 1% to 5%, the area fraction of a cementite phase present in a grain of the ferrite phase being 5% or less. Upon manufacture, a hot-rolled sheet or a cold-rolled sheet is heated to a temperature of 650° C. or higher at an average heating rate of 10° C./s or more, is held at a temperature of 700° C. to (Ac)° C. for ten seconds or more, is cooled to a temperature of 300° C. to 500° C. at an average cooling rate of 10° C./s to 200° C./s, is held at a temperature of 300° C. to 500° C. for 30 seconds to 300 seconds, and is then hot-dip galvanized.