The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 25, 2019

Filed:

May. 16, 2017
Applicant:

Citic Dicastal Co., Ltd., Qinhuangdao, CN;

Inventors:

Kaiqing Wang, Qinhuangdao, CN;

Hongbiao Li, Qinhuangdao, CN;

Xu Wang, Qinhuangdao, CN;

Changhai Li, Qinhuangdao, CN;

Yongwang Zhao, Qinhuangdao, CN;

Honghai Zhou, Qinhuangdao, CN;

Assignee:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B22C 9/28 (2006.01); B22D 18/04 (2006.01); B22C 9/06 (2006.01);
U.S. Cl.
CPC ...
B22C 9/28 (2013.01); B22C 9/065 (2013.01); B22D 18/04 (2013.01);
Abstract

The present disclosure provides a low-pressure cast aluminum wheel mold. The back cavity of a top mold () is divided into three parts: the back cavity in a rim area is open, and the wall thickness of the top mold is progressively increased by 15-25 mm from bottom to top; the back cavity in a spoke area is machined in a profile-followed manner, and the top mold has an equal wall thickness of 20-30 mm; at each R angle position where the rim is connected with a spoke, the top mold is provided with a boss (), the axial wall thickness of the boss () is 40-60 mm, and the radial wall thickness is 30-50 mm. A temperature gradient beneficial to progressive solidification of a casting is constructed; by designing an annular water cooling structure at the R angle where the rim is connected with the spoke, quick cooling on the hot spot is specifically realized, the cooling capability is stronger, the cooling range is more exact, bad influence on the adjacent thin-wall part is not produced, and smooth feeding of molten aluminum is ensured.