The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 04, 2019

Filed:

Feb. 09, 2017
Applicant:

Uacj Corporation, Chiyoda-ku, Tokyo, JP;

Inventors:

Yasunaga Itoh, Tokyo, JP;

Tomoki Yamayoshi, Tokyo, JP;

Assignee:

UACJ CORPORATION, Chiyoda-ku, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 35/00 (2006.01); B23K 35/28 (2006.01); B23K 35/02 (2006.01); C22C 21/06 (2006.01); C22C 21/02 (2006.01); B23K 1/00 (2006.01); B23K 1/20 (2006.01); B23K 35/38 (2006.01); F28F 21/08 (2006.01); B32B 15/01 (2006.01); C22C 21/00 (2006.01); B23K 101/14 (2006.01);
U.S. Cl.
CPC ...
B23K 35/286 (2013.01); B23K 1/00 (2013.01); B23K 1/0012 (2013.01); B23K 1/20 (2013.01); B23K 1/206 (2013.01); B23K 35/00 (2013.01); B23K 35/0238 (2013.01); B23K 35/38 (2013.01); B32B 15/016 (2013.01); C22C 21/00 (2013.01); C22C 21/02 (2013.01); C22C 21/06 (2013.01); F28F 21/084 (2013.01); F28F 21/089 (2013.01); B23K 2101/14 (2018.08); Y10T 428/12764 (2015.01);
Abstract

An aluminum alloy brazing sheet achieves a stable brazability equal to by brazing using a flux, even if an etching treatment is not performed on the brazing site. The aluminum alloy brazing sheet is used to braze aluminum in an inert gas atmosphere without using a flux and includes a core material and a filler metal, one side or each side of the core material being clad with the filler metal, the core material being formed of an aluminum alloy that includes 0.2 to 1.3 mass % of Mg, the filler metal including 6 to 13 mass % of Si and 0.004 to 0.1 mass % of Li, with the balance being aluminum and unavoidable impurities, a surface oxide film having been removed from the brazing sheet, and an oil solution that decomposes when heated at 380° C. or less in an inert gas having been applied to the brazing sheet.