The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 28, 2019

Filed:

Feb. 21, 2018
Applicant:

Joled Inc., Tokyo, JP;

Inventors:

Hideyuki Shirahase, Tokyo, JP;

Hiroyuki Ajiki, Tokyo, JP;

Jun Hashimoto, Tokyo, JP;

Masaki Nishimura, Tokyo, JP;

Assignee:

JOLED, INC., Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01L 51/52 (2006.01); H01L 27/32 (2006.01); H01L 51/50 (2006.01); H01L 51/56 (2006.01);
U.S. Cl.
CPC ...
H01L 51/5265 (2013.01); H01L 27/3244 (2013.01); H01L 51/5012 (2013.01); H01L 51/5076 (2013.01); H01L 51/5092 (2013.01); H01L 51/5218 (2013.01); H01L 51/5234 (2013.01); H01L 51/56 (2013.01); H01L 2227/323 (2013.01); H01L 2251/308 (2013.01); H01L 2251/5315 (2013.01); H01L 2251/558 (2013.01);
Abstract

An organic EL element includes an anode, a light emitting layer, a functional layer, a cathode, and a low refractive index layer. The light emitting layer is disposed above the anode. The functional layer is disposed on and in contact with the light emitting layer and includes a first metal. The cathode is disposed on and in contact with the functional layer and is made of a light transmissive metal oxide. The low refractive index layer is disposed on and in contact with the cathode. Refractive index of the low refractive index layer is smaller than refractive index of the cathode, film thickness of the functional layer is from 15 nm to 35 nm, and a distance between an anode-side surface of the light emitting layer and an interface between the cathode and the low refractive index layer is 110 nm or greater.